Highly selective collector for copper sulfide minerals, especially chalcopyrite and bornite.
Excellent flotation performance at low dosages, improving reagent economy and process efficiency.
Good tolerance to variations in pulp pH and temperature across typical concentrator operating ranges.
Reduced environmental impact compared to traditional xanthate-based collectors due to lower toxicity profile.
Stable emulsion formulation ensures consistent dispersion and dosage control in plant feed systems.
Copper-molybdenum porphyry ore flotation circuits.
Selective recovery of copper sulfides in complex polymetallic ores.
Regrind and cleaner circuit applications requiring high selectivity over iron sulfides.
Low-grade oxide-sulfide mixed ore processing where enhanced sulfide mineral response is critical.
| Chemical Type | Thiophosphinic acid derivative (alkyl dithiophosphinate) |
| Product Form | Liquid emulsion |
| Appearance | Ambient-stable, light amber to pale yellow homogeneous liquid |
| Primary Applications | Copper sulfide flotation, especially in Cu-Mo separation |
| Key Features | High selectivity, low dosage requirement, pH robustness (5.5–10.5) |
| Benefits | Improved grade/recovery balance, reduced reagent consumption, lower tailings sulfur content |
| Storage Temperature Range | 5 °C to 40 °C (avoid freezing and prolonged exposure >45 °C) |
| Shelf Life | 24 months from date of manufacture when stored under recommended conditions |